How Do You Specify Powder Coating?

Fabex Engineering Team October 29, 2026
How Do You Specify Powder Coating? — Powder coated sheet metal parts

How Do You Specify Powder Coating?

A usable powder coating specification has eight fields: coating chemistry, colour reference, gloss level, film thickness range, pretreatment, masking, substrate, and acceptance criteria. A colour name on its own is not a specification — “black” tells a coater almost nothing about what to apply, and two suppliers will interpret it differently.

Film thickness for decorative and functional powder work commonly lands somewhere around 60–120 µm, but the correct figure depends on the product, the service environment and the standard being worked to. The eight fields below are what remove the ambiguity.

1. Coating chemistry

Powder coatings are not interchangeable. The main families, and what they are chosen for:

Chemistry Typical use Consideration
Polyester Exterior and architectural work Good UV stability; the usual choice for outdoor equipment
Epoxy Interior, chemical resistance Excellent mechanical and chemical performance, poor UV stability — chalks outdoors
Epoxy-polyester hybrid Interior decorative work Balance of cost and performance, indoor only
Polyurethane Where appearance and durability both matter Higher cost
Fluoropolymer Severe exposure, long-life architectural Highest cost, specified where the service life demands it

Specifying “powder coat” without naming a chemistry means the coater chooses, and the choice will be driven by what is on the shelf. If the part will live outdoors, saying so — and asking for a chemistry suitable for exterior exposure — matters more than the colour.

2. Colour reference

The colour must be a reference, not a description:

  • A standard reference — RAL, Pantone, or a British Standard number — is the usual minimum.
  • A physical master sample is better where colour is critical, because it captures the effect of the substrate, the pretreatment and the gloss together.
  • Say who holds the master and how long it is valid. A master sample that lives in a drawer and has faded for three years is not a reference.

One point that catches people out: the same reference will not look identical over different substrates or pretreatments, or at a different gloss level. If two parts must match visually, they must share the full specification, not just the colour.

The RAL Classic references that come up most often on fabricated sheet metal — and the gloss and texture terms that go with them — are listed in the RAL powder coating colour and finish reference.

3. Gloss level

Gloss is specified in gloss units, typically measured at 60°. Common bands:

  • Matt — roughly under 10–20 units. Hides surface imperfections; shows handling marks and fingerprints differently from gloss.
  • Satin / semi-gloss — commonly around 30–50 units.
  • Gloss — commonly 70–90 units. Shows every surface defect; unforgiving on large flat panels.

Gloss is one of the most common sources of “this does not match” disputes, because it is rarely specified and is very visible when it differs between batches or between parts of an assembly.

4. Film thickness

Thickness is specified as a range, not a single number, and it is measured — usually with a magnetic or eddy-current gauge, often at several points per part.

  • Decorative and general functional work commonly sits around 60–120 µm.
  • Below the range, corner coverage and corrosion protection suffer — coating pulls back from sharp edges during cure.
  • Above the range, the coating can become brittle, chip more readily, and lose impact resistance; it also fills threads and close-tolerance features.

Thickness is not a case where more is better. A specification that says “minimum 100 µm” and nothing else will produce parts that fail impact tests.

5. Pretreatment

Pretreatment is what the coating adheres to, and it is often the difference between a finish that lasts and one that peels.

  • Degrease and clean is the absolute minimum.
  • Chemical conversion coating (for example a chromate-free conversion coat or a phosphate) is standard for ferrous parts and adds both adhesion and corrosion resistance.
  • Blast or mechanical preparation where a surface profile is needed.
  • For aluminium, a chromate-free conversion coating is normal; for galvanised steel, a suitable pretreatment is essential because zinc surfaces behave differently.

The pretreatment should be specified by outcome — what it is for, and to what standard — rather than by process name alone, since processes differ between coaters.

6. Masking

Everything that must not be coated needs to be identified, because coating a mating surface, thread or contact is difficult to undo:

  • Threaded holes and studs — powder in a thread means chasing or retapping.
  • Grounding and bonding points — a coated surface is an insulator, which breaks the electrical path the design assumes.
  • Mating and sealing faces — coating thickness changes fit and gasket compression.
  • Close-tolerance bores and locating features.
  • Hinge points, sliding surfaces and pressed-in inserts.

Masking is a cost item and a quality risk, so it should be listed explicitly on the drawing rather than left to a general note.

7. Substrate

The substrate determines what is possible with the rest of the specification:

  • Cold-rolled steel is the most straightforward.
  • Galvanised and zinc-coated steels need a pretreatment suited to zinc, and can show outgassing defects if the zinc is not properly prepared.
  • Aluminium needs its own pretreatment and, if it is also anodised elsewhere on the part, clear masking instructions.
  • Previously coated surfaces should be declared, since recoating over an unknown coating is a common cause of adhesion failure.
  • Welds and cut edges should be considered — a weld bead draws coating away from sharp transitions, and a bare cut edge is a corrosion initiation point.

8. Acceptance criteria

Finally, say how the finish will be judged and by what method.

  • Colour and gloss against the master sample, under stated lighting.
  • Thickness — what instrument, how many readings, on which surfaces.
  • Adhesion — a cross-hatch or pull-off test to a named standard, if required.
  • Impact or flexibility — relevant where parts are formed or handled after coating.
  • Salt spray or corrosion testing — only if the application genuinely requires it, since it is slow and expensive.
  • Appearance — a visual standard with a defined viewing distance and lighting. “No visible defects” is not testable; a defined defect size limit and viewing condition is.

If a test is required, the standard it is performed to should be named. An acceptance criterion without a method is an argument waiting to happen.

The most common omissions

In practice, these are the fields that go missing most often:

  1. No chemistry — “powder coat” with no product family.
  2. A colour name instead of a reference.
  3. No gloss level.
  4. A single thickness figure rather than a range.
  5. No pretreatment specified.
  6. No masking list, particularly around grounding points and threads.
  7. No master sample, or one that is no longer representative.
  8. No acceptance criteria, so the finish is judged on opinion.

Each of these is a sentence on a drawing, and each of them removes a class of dispute.

The wider list of drawing requirements is in the sheet metal drawing requirements and DFM checklist.


Related reading: sheet metal powder coating techniques and applications, powder coating vs wet painting vs anodizing, and sheet metal painting and powder coating.

Request a Free Quote

Send the project details below for drawing review and quotation planning.

By submitting you agree to our Privacy Policy.

We respect your privacy. Your information is secure and will never be shared.