Sourcing to Australian Standards: AS/NZS Grades, Coatings and What Actually Ships

Fabex Engineering Team September 16, 2026
Sourcing to Australian Standards: AS/NZS Grades, Coatings and What Actually Ships — MIG and TIG welding of sheet metal assemblies

Sourcing to Australian Standards: AS/NZS Grades, Coatings and What Actually Ships

Australian and New Zealand drawings tend to carry two things a Chinese mill does not see every day: an AS/NZS product standard, and a coating class expressed in grams per square metre. Neither is exotic, but both need translating before a quote means anything.

Part 1 of this series covered the general substitution decision. This article is the Australian and New Zealand case: what the standards actually control, which parts of them are easy to match, and where an exact-match order stops being worth the money.

Standing caution. The cross-references below are procurement directions, not certifications. Confirm every one against a mill certificate and your engineer’s approval before a part is made.

What an AS/NZS drawing is really specifying

Four standards do most of the work in sheet metal work, and they specify different things:

Standard What it covers Practical meaning
AS/NZS 1397 continuously produced metallic-coated steel sheet and strip the everyday “galvanized / Zincalume” material: grade, coating type and coating class
AS/NZS 1594 hot-rolled steel flat products heavier hot-rolled sheet and plate for structural work
AS/NZS 3679.1 hot-rolled bars and sections structural sections, not sheet — but the grade names are shared, which causes confusion
AS/NZS 4680 hot-dip galvanized coatings applied after fabrication the coating on a finished part, dipped after welding and drilling

That last one is the one buyers most often mean without saying it. A part made from pre-coated Z275 sheet and a part hot-dip galvanized after fabrication are different products with different corrosion behaviour at cut edges, welds and threads — and very different lead times.

Coating classes: the number that matters

AS/NZS 1397 expresses coating as a class letter and a mass in grams per square metre — Z275, Z350, AZ150, ZA. The letter is the coating alloy:

  • Z — zinc. The ordinary galvanized coating.
  • AZ — 55% aluminium-zinc. Better cut-edge and long-term performance in many environments; what “Zincalume” describes.
  • ZA — zinc-aluminium, a middle family.
  • ZM / ZMA — zinc-aluminium-magnesium, the newest family, with noticeably better edge protection than plain zinc.

The number is a coating mass, and the basis matters. A Z275 is a mass of 275 g/m², and in AS/NZS 1397 the class refers to the total coating on both surfaces. This is exactly where a substitution goes quietly wrong, because Chinese stock lists often quote coating per side. A “Z120 double-sided” is not a Z275.

If the drawing says The number to hold onto Commonly encountered equivalent
Z275 (galvanized) 275 g/m² total both faces SGCC with a matching coating mass; US G90
Z350 350 g/m² total heavy galvanized, often a special order in China
AZ150 (55% Al-Zn) 150 g/m² total AZ150 is internationally common; check the alloy, not just the number
ZM / ZMA (Zn-Al-Mg) as designated Zn-Al-Mg coil, e.g. Magnelis S250GD+ZM310, SGH340D+ZMA275

The practical rule: a Z275-class requirement is a normal, readily available sheet. A Z350-class requirement at low volume is where minimums appear, and where AZ150 or a Zn-Al-Mg coil may actually be the better engineering answer for the same money.

Grades: G300, G350 and what they really are

The Australian structural sheet grades most often written on a drawing are G300, G350, G450, G500 and G550 — the number is the minimum yield strength in megapascals. Designers also specify CA (cold-reduced, annealed) material for formed parts, and drawing-quality grades where a part is deeply formed.

In China, the same strength families are everywhere under different names:

Australian designation What it guarantees Chinese-mill families that usually hit the number
G300 / CA material ~300 MPa minimum yield SGCC/SECC general grades; Q355 territory in heavier gauges
G350 ~350 MPa minimum yield Q355B (GB/T 1591), S355JR (EN 10025-2)
G450 / G500 450–500 MPa minimum yield Q460 family, HSLA grades
G550 550 MPa minimum yield high-strength zinc-coated strip, usually a mill order
304 / 316 stainless austenitic stainless SUS304 / SUS316L — no translation needed
5052 aluminium Al-Mg sheet 5052 / EN AW-5052 — no translation needed

Two of these are easy and one is a trap:

  • G350 → Q355 / S355 is the routine substitution. Both families guarantee roughly 350 MPa minimum yield with comparable chemistry, and a mill certificate that states the yield is the evidence you need. Confirm the certified minimum, not the grade name.
  • G550 is genuinely a mill-order material. If a design depends on it, that is a programme decision, not a sourcing detail.
  • The trap is structural intent. If the part is a structural member designed to AS 4100 and welded to AS/NZS 1554, “equivalent strength” is not the whole requirement — the execution standard and welding qualification are part of the specification, and those are producer certifications, not material properties. A fabricator that does not hold them cannot make the claim by buying better steel.

Hot-dip galvanizing after fabrication

AS/NZS 4680 governs hot-dip galvanizing applied to a finished fabricated part: the steel is cleaned, dipped in molten zinc, and the coating forms on every surface including inside corners and cut edges. The standard sets coating mass classes and inspection requirements.

This is a different product from pre-coated sheet, and its advantage is exactly where pre-coated sheet is weakest: cut edges, welds and drilled holes get coated too, because the coating is applied after all that work.

The consequences for a drawing:

  • Drain and vent holes must be designed in. A sealed hollow section cannot be galvanized — the part traps air or molten zinc. This is a design rule, not a supplier preference.
  • Dimensional change at threads and precision fits; threads are usually cut or re-tapped after dipping, or protected.
  • Coating thickness adds time. After-fabrication galvanizing is a coordinated specialist process with its own lead time, not a stock material.
  • Appearance is not a cosmetic finish. Dipping produces a variable, spangled surface. If a face is visible, specify what is acceptable rather than discovering it at first article.

For outdoor parts in coastal Australia, the choice between heavier pre-coated sheet, an AZ-coated, a Zn-Al-Mg coil and after-fabrication dipping is a real engineering decision, and it is worth making explicitly rather than inheriting from a previous supplier’s habit.

Welding and the qualification question

Australian structural welding is governed by the AS/NZS 1554 series, which requires qualified welding procedures and welder qualification. That is a certification held by the fabricator, not a property of the material. A supplier can always buy the right steel; only a qualified fabricator can claim to weld to a structural welding standard.

If your part is structural and the specification invokes AS/NZS 1554, ask directly which procedures and qualifications the fabricator holds, and ask for the documentation. If the part is a non-structural bracket or enclosure, saying so removes an unnecessary requirement from the quotation and often removes cost with it.

What to put on the drawing for an Australian job

  • The exact standard and grade — “AS/NZS 1397 CA Z275, 1.5 mm” rather than “galvanized 1.5”.
  • Coating on a stated basis — total both faces, and whether any cut-edge protection is expected.
  • Whether the part is structural — and if so, which execution or welding standard applies.
  • Thickness tolerance class, not just nominal thickness.
  • The end-use environment — inland, coastal, marine splash. This is what decides whether Z275 is enough or the answer is a heavier coating system.
  • The certificate you need — mill certificate, a specific certificate type, or third-party testing.

The honest summary

An Australian specification is usually satisfiable in China at two levels. The material and coating are straightforward: the grade families exist and the coating classes can be matched numerically. The execution and certification are not automatic: structural welding qualifications, after-fabrication galvanizing to AS/NZS 4680, and exact dual-certified AS/NZS product standards all sit with specific suppliers and specific programmes, and at low volume they carry a mill minimum.

Deciding which of those you actually need is where the money is. The next two parts cover the same question in the European and US systems, where the certificate language changes but the decision does not.

If you have an AS/NZS drawing and want to know what the practical material answer is at your quantity, send it over with the environment and the certificate requirement stated.

Request a Free Quote

Send the project details below for drawing review and quotation planning.

By submitting you agree to our Privacy Policy.

We respect your privacy. Your information is secure and will never be shared.